Capsulization


Reading time ( words)

Since lead-free implementation, concerns about tin whiskers have intensified. For the past 12 years, studies and research by various laboratories and organizations have delivered burgeoning reports and papers, and my column has devoted an entire series to this subject. This article aims to capsulize the important areas of the subject. (Note: For expression, “whisker” is used as both noun and verb.)

The tin whisker issue and its potential mishaps have been recognized for more than six decades in electronic, electrical, and industrial applications. Some metals are prone to whiskering, or protruding from the surface of the substrate. In addition to tin, the metals that have exhibited whiskers include zinc, cadmium, silver, gold, aluminum, copper, lead, and others.

The whiskering phenomenon is distinct and unique. It is the result of a process different from other known phenomena (e.g., dendrites). And tin whisker and tin pest are separate metallurgical phenomena (SMT Magazine, May 2013). However, whiskers share commonality with dendrites in two aspects: Both are the result of a physical metallurgical process, thus following the science of physical metallurgy; and both could cause a product failure.

Uncertainty about tin whisker growth is most insidious. Stock markets do not like uncertainty, nor does the electronics industry. Our effort is to alleviate the uncertainty.

Practical Criteria

As some metals can whisker when accommodating conditions are met, the goal should be set with the differentiation between whisker-resistant and whisker-proof.

Overall, for testing or evaluation of the whisker propensity of a system, the key questions to be addressed are, is the system whisker-prone or whisker-resistant (not whisker-proof), and how does the system’s whisker resistance stand in reference to the intended benchmark?

Read the full article here.


Editor's Note: This article originally appeared in the July 2014 issue of SMT Magazine.

Share

Print


Suggested Items

High-reliability, Low-temperature Solder Alloys

05/18/2020 | Dr. Pritha Choudhury, MacDermid Alpha Electronics Solutions
Increased digitalization and greater connectivity have been driving miniaturization and more complex and integrated designs in electronics. As the real estate on PCBs shrinks, so does the size of packages. However, the drive for finding design solutions for increased performance has continued to expand. The solder joint is an essential part of assemblies for electronic devices as it provides electrical, thermal, and mechanical connections. Therefore, soldering materials have been evolving to enable such a technological revolution.

Process Ionic Contamination Test (PICT) Standard Roundtable With Industry Experts

04/22/2020 | I-Connect007
With standards committees set to release the first of four new test standards, industry experts discussed the process ionic contamination test (PICT) standard, which was recently approved by the IEC for publication. Roundtable participants included Teresa Rowe, senior director of assembly and standards technology at IPC, Graham Naisbitt, chairman and CEO of Gen3, Jason Keeping, corporate process development at Celestica, and Doug Pauls, principal materials and process engineer at Collins Aerospace.

Joe Fjelstad Breaks Down His Occam Process

03/04/2020 | I-Connect007 Editorial Team
Joe Fjelstad recently met with the I-Connect007 Editorial Team to discuss the potential benefits of his Occam process for solderless assembly. This technique allows assembly of the PCB without the risks associated with traditional surface-mount processes, such as solder joint failure. Has the time come for the industry to embrace Occam?



Copyright © 2020 I-Connect007. All rights reserved.